Our Online Store Is Now Available For Ordering.

Sink Marks in Injection Molding: Causes and Solutions

injection molding machine maintenance

Table of Contents

Sink marks show up where a part is thick. Here is why they form, and how process, mold, design and material each play a part in fixing them.

Sink marks are the small depressions that appear on a part’s surface, usually opposite a rib, boss or other thick section. On a textured interior part they may be nearly invisible. On a glossy, cosmetic surface they can be grounds for rejecting the whole lot.

Texas Injection Molding describes sink marks as surface depressions caused by localized volumetric shrinkage in thick sections during cooling. Understanding that one sentence is most of the battle. This article is part of our injection molding defect library; for every common defect in one place, see Common Injection Molding Defects and How to Fix Them.

Why sink marks form

Plastic shrinks as it cools. The outer skin against the mold cools and solidifies first. The core of a thick section stays molten longer, and as it cools and shrinks, it pulls on the skin. If the skin is still soft enough to move, it gets pulled inward and you see a sink mark. If the skin is already rigid, the shrinkage stays inside the part as a void instead.

That is why sink marks cluster in predictable places: at the base of ribs, opposite bosses, at thick corners and anywhere the wall is heavier than the nominal thickness around it. Researchers modeling sink marks at the base of ribs have shown that sink depth depends on both the part’s geometry and the molding parameters used to make it.

The four causes of sink marks

1. Part design: thick sections

Thick walls and isolated heavy sections are the root of most sink marks. Texas Injection Molding identifies bosses or ribs thicker than 65% of the nominal wall as a common cause and recommends sizing ribs at roughly 50% to 65% of the main wall thickness. RJC Mold adds coring out solid sections, smoothing transitions from thick to thin, and setting a maximum wall thickness during design.

2. Packing: not enough material pushed in while the part cools

Holding pressure is what compensates for shrinkage. It packs additional material into the cavity as the part cools. Too little packing pressure or a gate that freezes too early both leave a thick section without that extra material. RJC Mold notes that on long flow paths, pressure may simply not reach the sink area before the gate freezes.

A few checks help separate a packing problem from the rest:

  • Is there a cushion? If the screw bottoms out, there is no material left to pack with, and raising holding pressure does nothing.
  • Is the hold time long enough? If hold ends before the gate freezes, material can flow back out. Weighing parts at increasing hold times shows when weight stops rising. Our article on holding pressure and part weight walks through this.
  • Is the sink far from the gate? Distance from the gate makes packing harder.

3. Cooling: uneven mold temperatures

An area of the mold that runs hotter keeps that section of the part molten longer, and that section shrinks more. RJC Mold notes that when cooling is the cause, adding holding pressure usually helps little. Look at cooling line layout, water flow and the temperature of each mold half.

4. Material: some resins shrink more

Material choice changes how much shrinkage you are fighting. RJC Mold rates the sink tendency of polypropylene and polyethylene as high, nylon as medium to high, ABS as medium and polycarbonate as low. Semi-crystalline resins generally shrink more than amorphous ones. Switching material is rarely the first fix, but it explains why a part that molds cleanly in one resin sinks in another. Our guide on choosing the right plastic resin covers the trade-offs.

Fixes in the order we would try them

Step What to do Why
1. Confirm the cushion Make sure the screw is not bottoming out No cushion means no packing
2. Raise packing pressure and extend hold time Increase in steps and weigh parts Pushes more material into shrinking sections
3. Check mold temperature balance Measure both mold halves and problem areas Hot spots shrink more
4. Adjust mold temperature Increasing mold temperature is one listed fix Changes how the skin and core cool
5. Review the gate Place the gate nearer thick areas or enlarge it Helps packing reach the sink area
6. Revise the design Thin ribs and bosses, core out thick sections Removes the source of the shrinkage
Sink marks or voids? Raising packing pressure can sometimes turn a sink mark into an internal void, because the shrinkage still has to go somewhere. If a cosmetic fix creates a structural problem, the real solution is in the part design or the cooling.

Where the machine fits in

Sink marks are often a packing problem, and packing depends on a machine that holds pressure and position consistently from shot to shot. LOG Injection Molding Machines’ S-9 Series provides real-time control over injection speed, pressure and screw position with closed-loop control, which helps keep cushion and holding pressure stable across a run.

Machines mentioned in this article

S-9 Servo Series
Real-time control of injection speed, pressure and screw position with closed-loop control
View machine →
S-8 Servo Series
Multi-step pressure, speed and time control for plasticizing
View machine →
Virtus Equipment Direct
Replacement parts for LOG Injection Molding Machines, including heater bands and electrical components
View machine →

Need more consistent packing?

LOG Injection Molding Machines can help you match a press with the injection control your parts need.

Frequently asked questions

What causes sink marks in injection molding?
Sink marks are caused by localized shrinkage in thick sections as the part cools. Thick walls, oversized ribs and bosses, too little packing, early gate freeze, uneven cooling and high-shrinkage materials all contribute.

How thick should ribs be to avoid sink marks?
Texas Injection Molding recommends sizing ribs at roughly 50% to 65% of the nominal wall thickness and identifies ribs or bosses thicker than 65% of the wall as a common cause of sink.

Does increasing holding pressure fix sink marks?
Often, when the cause is insufficient packing. When the cause is uneven cooling, adding holding pressure usually helps little. It also only works if there is a cushion left to pack with.

Which plastics are most prone to sink marks?
RJC Mold rates polypropylene and polyethylene as high sink tendency, nylon as medium to high, ABS as medium and polycarbonate as low.

What is the difference between a sink mark and a void?
Both come from shrinkage in a thick section. If the surface skin is still soft, it is pulled inward as a sink mark. If the skin is already rigid, the shrinkage forms a void inside the part.

Keep reading

error: Content is protected !!